MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® XE 4116 nat PA1010-GF55  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted parts in complex designs. Grilamid XE 4116 natural has the following product profile:
  • Polymer based primarily on renewable resources
  • High stiffness and strength
  • Excellent impact and notched impact strength
  • Improved warpage performance
  • Improved flowability
  • Easy processing
  • Excellent surface finish
  • Good UV and chemical resistance
  • Improved paint adhesion
Grilamid XE 4116 natural is suitable for the manufacturing of production of moldings in the application fields of:
  • Electronic devices
  • Automotive structural parts
  • Mechanical engineering, industry goods
  • Sports & leisure goods

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccISO 1183
Water Absorption 1.7 %ISO 62
Moisture Absorption 0.900 %ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 215 MPaconditioned; ISO 2039-1
 230 MPadry; ISO 2039-1
Tensile Strength at Break 180 MPaconditioned; ISO 527-1/-2
 210 MPadry; ISO 527-1/-2
Elongation at Break 2.5 %dry; ISO 527-1/-2
 2.5 %conditioned; ISO 527-1/-2
Tensile Modulus 16500 MPaconditioned; ISO 527-1/-2
 17500 MPadry; ISO 527-1/-2
Charpy Impact Unnotched 75.0 kJ/m²conditioned; ISO 179/1eU
 90.0 kJ/m²dry; ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
conditioned; ISO 179/1eU
 85.0 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²conditioned; ISO 179/1eA
 20.0 kJ/m²dry; ISO 179/1eA
 14.0 kJ/m²
@Temperature -30.0 °C
conditioned; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmdry; IEC 60093
 1.00e+12 ohm-cmconditioned; IEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Strength 36.0 kV/mmdry; IEC 60243-1
 36.0 kV/mmconditioned; IEC 60243-1
Comparative Tracking Index 600 Vconditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
Melting Point 200 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 °Clong term; EMS
 150 °Cshort term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 185 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 150 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Compressed air systems
 Exterior
 Hydraulic systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Lighting
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesBio based Polyamide
 Improved flowability and demolding
Special CharacteristicsHigh impact or impact modified
 Improved UV resistance (outdoor use)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® 1SVX-65H nat PA1010-GF65
EMS-Grivory Grilamid® 1SVX-50H nat PA1010-GF50
RTP Company RTP 2099 X 126216 D Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 59% Renewable Resource Content
EMS-Grivory Grilamid® XE 4181 nat PA1010
EMS-Grivory Grilamid® XE 4180 nat PA1010

PGRH135 / 156844

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.