MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ FR Resin RCM6134 Polycarbonate + ABS (PC+ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY RCM6134 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1.0mm. Developed for thin wall applications that require high flow and high stiffness performance. Limited availability and restricted color only.

Features: Flame Retardant,Non-Chlorinated,Non-Brominated,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Moisture Absorption 0.0400 %Injection Molding
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 44.0 MPa5 mm/min; ASTM D638
 48.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 54.0 MPa5 mm/min; ASTM D638
 56.0 MPa5 mm/min; ISO 527
Elongation at Break 70 %5 mm/min; ASTM D638
 75 %5 mm/min; ISO 527
Elongation at Yield 3.4 %5 mm/min; ISO 527
 3.5 %5 mm/min; ASTM D638
Tensile Modulus 3100 MPa5 mm/min; ASTM D638
 3100 MPa1 mm/min; ISO 527
Flexural Strength 90.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 95.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 3100 MPa1.3 mm/min, 50 mm span; ASTM D790
 3100 MPa2 mm/min; ISO 178
Izod Impact Notched 300 JASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²80*10*3; ISO 180/1A
Charpy Impact, Notched 11.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 52.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=3.00 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 80.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 V-1
@Thickness >=0.800 mm
UL 94
 V-0
@Thickness >=1.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 245 - 275 °C
Zone 2 220 - 265 °C
Zone 3 245 - 275 °C
Melt Temperature 245 - 275 °CInjection Molding
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 - 90.0 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80039 / 287986

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.