This modified cast polyamide PA 6 G is easily identifiable by its blue colouring. It has a higher toughness, flexibility, and fatigue strength than unmodified PA 6 G. These characteristics make this type ideal for gear wheels, pinions, and toothed racks.Information provided by Angst + Pfister |