MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PPS GF SL PPS + glass fibre + solid lubricant
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler

Material Notes: This fibre-reinforced type of polyphenylene sulphide has an integral solid lubricant. It has an exceptional combination of properties with regard to its wear resistance, mechanical load-bearing capacity, and dimensional stability, even when exposed to chemicals and high temperatures. This material is used wherever other technical plastics such as PA, POM, PET, PEI, and PSU are no longer sufficient or where a more cost-effective alternative to PI, PEEK, or PAI is sought in less challenging high-tech applications. Thanks to the homogeneously distributed, integral solid lubricant, PPS GF SL has excellent wear resistance and a low coefficient of sliding friction. It is able to overcome the disadvantages of unfilled PPS (high coefficient of sliding friction) and of glass fibre reinforced PPS (early wear of mating surface) in the case of sliding elements. Naturally, these characteristics combined with exceptional chemical resistance open up a wide range of possible applications in all possible industrial sectors, e.g. industrial drying furnaces and ovens for food processing, devices for chemical processing, and electrical insulation systems.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccDIN EN ISO 1183-1
Water Absorption 0.010 %
@Time 86400 sec
DIN EN ISO 62
 0.020 %
@Time 346000 sec
DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 160 MPaDIN EN ISO 2039-1
Tensile Strength at Break 78.0 MPa5 mm/min; DIN EN ISO 527
Tensile Strength 78.0 MPaDIN EN ISO 527
Elongation at Break 3.5 %5 mm/min; DIN EN ISO 527
Modulus of Elasticity 4.00 GPaDIN EN ISO 527
Compressive Strength 33.0 MPa
@Strain 1 %,
Load 1.02 kg
5 mm/min; EN ISO 604
 65.0 MPa
@Strain 2 %,
Load 1.02 kg
5 mm/min; EN ISO 604
Charpy Impact Unnotched 25.0 kJ/m²DIN EN ISO 179-1eU
Charpy Impact, Notched 4.00 kJ/m²DIN EN ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmANSI/ESD STM 11.11
Dielectric Constant 3.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength 24.0 kV/mmIEC 60243
Dielectric Loss Index 0.0030
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 100 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
Thermal Conductivity 0.300 W/m-K
Melting Point 280 °CISO 11357-3
Maximum Service Temperature, Air 220 °Clong term
 260 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 115 °CDIN EN ISO 75 / A
Minimum Service Temperature, Air -20.0 °C
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 
Descriptive Properties
Colordark blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP057 / 250555

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.