MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
PolyMirae Moplen HP562T Fiber (Spunbond) Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Moplen HP562T is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562T is a homopolymer particularly suitable for fine denier spunbonded nonwovens. Moplen HP562T resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520.

Features: Excellent spinnability; Excellent drawability; Fine Denier; Odorless; Narrow molecular weight distribution; Anti-gas Fading

Applications: Diaper and Sanitary Napkin; Agriculture; Shopping Bag; Apparel Cover; Wet Tissues

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ASTM D785
Tensile Strength, Yield 380 kg(f)/cm²ASTM D638
Elongation at Yield 8.0 %ASTM D638
Flexural Modulus 15000 kg(f)/cm²ASTM D790
Izod Impact, Notched 2.00 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °CASTM D648
Vicat Softening Point 150 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Moplen HP563S Fiber (Spunbond) Grade Polypropylene
Total PPR 7860 Controlled Rheology Grade Propylene Copolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns and Extrusion Coating
Total PPH 3866 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns, and Extrusion Coating
Total PPH 3764 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics and Multifilament Yarns
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene

PMIRAE45 / 53157

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.