MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Radici Radilon® S RV350W 333 BK Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: PA6 35% glass fiber reinforced, injection molding grade. Heat stabilization. Black color.

Suitable for parts requiring high stiffness, good mechanical resistance and excellent heat aging properties retention.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccDAM; ISO 1183
Water Absorption 6.4 %
@Thickness 2.00 mm,
Time 86400 sec
Immersion @ 23°C; ISO 62
Moisture Absorption 1.80 %
@Thickness 2.00 mm,
Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 115 MPa5mm / min. Conditioned; ISO 527-2/1A
 180 MPa5mm / min. DAM; ISO 527-2/1A
Elongation at Break 3.1 %5 mm / min. DAM; ISO 527-2/1A
 7.0 %5 mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 6900 MPa1mm / min. Conditioned; ISO 527-2/1A
 10800 MPa1mm / min. DAM; ISO 527-2/1A
Flexural Strength 175 MPa5 mm / min. Conditioned; ISO 527-2/1A
 275 MPa2mm / min. DAM; ISO 178
Flexural Modulus 6.80 GPa5 mm / min. Conditioned; ISO 527-2/1A
 10300 MPa2mm / min. DAM; ISO 178
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 11.0 J/cm²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1e/A
 25.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1e/A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohmDAM; 500V.; IEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75/2Af
Vicat Softening Point 210 °CISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
Automotive Interior; ISO 3795
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 280 °CInjection Molding
Mold Temperature 80.0 - 90.0 °C
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6965 / 293470

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.