Molding Grade PCFR w/ UV and Release, All Colors but Clear FR PC. Polycarbonate (PC), furnished as pellets, (All Colors but Clear). May be used to produce molded or extruded articles or as a component of other industrial products.Information provided by Star Plastics. |