MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound KI001 Acetal (POM) Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: LNP LUBRICOMP KI001 compound is based on POM (Acetal) resin containing silicone. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.025 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 44.0 MPa5 mm/min; ISO 527
Tensile Modulus 2500 MPa1 mm/min; ISO 527
Flexural Strength 65.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2000 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.20 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 57.0 kJ/m²80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.20ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.30ASTM D3702 Modified: Manual
K (wear) Factor 66.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 105 µm/m-°C
@Temperature -30.0 - 30.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 123 µm/m-°C
@Temperature -30.0 - 30.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 
Processing PropertiesOriginal ValueComments
Zone 2 190 - 210 °C
Zone 3 200 - 220 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80838 / 288785

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.