MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LEXAN™ Copolymer FST3403 Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior applications (category R6). It also meets requirements of DIN5510-2, NFPA-130 and PN-K-02511 standards. Available in opaque colors.

Features: Low Smoke and Toxicity

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Viscosity 10 cP
@Load 1.20 kg,
Temperature 300 °C
10 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
Melt Flow 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
12 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psi50 mm/min; ASTM D638
 70.0 MPa10200 psi50 mm/min; ISO 527
Tensile Strength, Yield 77.0 MPa11200 psi50 mm/min; ASTM D638
 77.0 MPa11200 psi50 mm/min; ISO 527
Elongation at Break 80 %80 %50 mm/min; ASTM D638
 80 %80 %50 mm/min; ISO 527
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
 6.0 %6.0 %50 mm/min; ISO 527
Tensile Modulus 2.60 GPa377 ksi5 mm/min; ASTM D638
 2.60 GPa377 ksi1 mm/min; ISO 527
Flexural Strength 110 MPa16000 psiyield, 2 mm/min; ISO 178
 115 MPa16700 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.50 GPa363 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.70 GPa392 ksi2 mm/min; ISO 178
Izod Impact Notched 130 J95.9 ft-lbASTM D256
 90.0 J
@Temperature -30.0 °C
66.4 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²80*10*4; ISO 180/1A
 13.0 kJ/m²6.19 ft-lb/in²80*10*3; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NBNBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 1.40 J/cm²6.66 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 80.0 J59.0 ft-lbASTM D3763
Impact Test 125 J92.2 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 104 °C
@Thickness 3.20 mm
219 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 93.0 °C
@Thickness 3.20 mm
199 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 114 °C237 °FRate B/50; ISO 306
 114 °C237 °FRate B/50; ASTM D1525
 115 °C239 °FRate B/120; ISO 306
Smoke Density <= 150<= 150DS-4, 50 kW/m2, 3mm; ISO 5659-2
 <= 300<= 300VOF4, 50 kW/m2, 3mm; ISO 5659-2
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 285 °C473 - 545 °F
Zone 2 240 - 280 °C464 - 536 °F
Zone 3 250 - 290 °C482 - 554 °F
Melt Temperature 250 - 290 °C482 - 554 °FInjection Molding
Mold Temperature 50.0 - 80.0 °C122 - 176 °F
Drying Temperature 95.0 - 100 °C203 - 212 °FInjection Molding
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
Fire Safety Hazard Level - Requirement set R6HL3EN 45545-2:2013
Heat release, MAHRE, 50 kW/m2, 3 mm<60 kW/m²ISO 5660-1
Smoke toxicity, CITG (8 min), 50 kW/m2, 3 mm0.1ISO 5659-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80246 / 288193

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.