MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX830 Polyphenylene Ether + PA (PPE+Nylon) (Asia)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 830 resin is a 30% glass reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade has high stiffness (flexural modulus 8200 MPa), excellent chemical resistance, and high heat resistance. NORYL GTX GTX830 resin is an excellent candidate for a wide variety of applications including automotive under the bonnet applications and water meter housings.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,High Heat Resistance,Good Stiffness,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Density 1.328 g/ccASTM D792
Moisture Absorption 0.0700 %Injection Molding
 0.500 %23°C/50% RH/24 hrs; ASTM D570
Moisture Absorption at Equilibrium 1.0 %23°C/50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0065 - 0.0085 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength at Break 158 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 151 MPa5 mm/min; ASTM D638
Elongation at Break 7.0 %5 mm/min; ASTM D638
Flexural Strength 248 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 8580 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 106 JASTM D256
 80.0 J
@Temperature -30.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 30 - 60 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.8 - 30.6 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 254 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 248 °CRate B/50; ASTM D1525
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 305 °C
Zone 2 270 - 305 °C
Zone 3 275 - 305 °C
Melt Temperature 280 - 305 °CInjection Molding
Mold Temperature 75.0 - 120 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %minimum
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82149 / 290096

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.