MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo Celanex® 2003-5FC PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Product Description: Celanex 2003-5FC is a general purpose, unreinforced polybuytlene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 2003-5FC is a medium to high flow material that contains an internal lubricant and nucleant.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Additive: Mold Release

Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183
Water Absorption 0.020 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.45 %ISO 62
Maximum Moisture Content 0.020
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.018 - 0.020 cm/cmISO 294-4
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8270 psiISO 527-2/50
Tensile Strength, Yield 9140 psiISO 527-2/50
Elongation at Break 15 %Nominal; ISO 527-2/50
Elongation at Yield 4.0 %ISO 527-2/50
Tensile Modulus 392000 psiISO 527-1
Flexural Strength 11600 psiISO 178
Flexural Modulus 370000 psiISO 178
Charpy Impact Unnotched 62.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eU
 64.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eU
Charpy Impact, Notched 2.10 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 2.40 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 61.0 µin/in-°FISO 11359-2
Melting Point 437 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 320 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 140 °FUnannealed; ISO 75-2/A
Vicat Softening Point 374 °FISO 306/B50
Glass Transition Temp, Tg 140 °FISO 11357-2
Flammability, UL94 HB
@Thickness 0.787 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 122 °FHopper
 482 - 500 °FHot Runner
Feed Temperature 446 - 464 °FInjection
Rear Barrel Temperature 446 - 464 °F
Middle Barrel Temperature 464 - 482 °F
Front Barrel Temperature 473 - 491 °F
Nozzle Temperature 482 - 500 °F
Zone 4 482 - 500 °FInjection
Melt Temperature 464 - 500 °F
Mold Temperature 158 - 194 °F
Drying Temperature 248 - 266 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6169 / 310862

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.