MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Stratasys® Diran 410MF07 Nylon-based thermoplastic FDM 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Diran™ 410MF07 is a nylon-based thermoplastic FDM® material, mineral-filled 7% by weight. It demonstrates very good toughness and impact strength combined with resistance to hydrocarbon-based chemicals. Its smooth, lubricious surface quality offers low sliding resistance. Typical applications include jigs, fixtures and other forms of general manufacturing tooling, and is particularly effective for applications needing a non-marring interface between the tool and the workpiece.

Information provided by Stratasys.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccXY Orientation; ASTM D792
 1.16 g/ccXZ/ZX Orientation; ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPaZX Orientation; ASTM D638
 40.0 MPaXZ Orientation; ASTM D638
Tensile Strength, Yield 45.0 MPaXZ Orientation; ASTM D638
Elongation at Break 3.1 %ZX Orientation; ASTM D638
 12 %XZ Orientation; ASTM D638
Elongation at Yield 4.26 %XZ Orientation; ASTM D638
Modulus of Elasticity 1.46 GPaZX Orientation; ASTM D638
 1.69 GPaXZ Orientation; ASTM D638
Flexural Strength 45.0 MPaZX Orientation; ASTM D790, Procedure A
 60.0 MPa
@Strain 5.0 %
XZ Orientation; ASTM D790, Procedure A
Flexural Modulus 1.47 GPaZX Orientation; ASTM D790, Procedure A
 1.85 GPaXZ Orientation; ASTM D790, Procedure A
Flexural Strain at Break 3.1 %ZX Orientation; ASTM D790, Procedure A
Compressive Yield Strength 75.0 MPaXZ Orientation; ASTM D695
 160 MPaZX Orientation; ASTM D695
Compressive Modulus 1.45 GPaZX Orientation; ASTM D695
 1.54 GPaXZ Orientation; ASTM D695
Izod Impact, Notched 27.0 J/mZX Orientation; ASTM D256, ASTM D4812
 380 J/mXZ Orientation; ASTM D256, ASTM D4812
Izod Impact, Unnotched 140 J/mZX Orientation; ASTM D256, ASTM D4812
 1415 J/mXZ Orientation; ASTM D256, ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.50e+15 ohm-cmXY Orientation; ASTM D257
 >= 1.50e+15 ohm-cmXZ/ZX Orientation; ASTM D257
Dielectric Constant 2.85
@Frequency 2.00e+6 Hz
XY Orientation; ASTM D150
 2.95
@Frequency 2.00e+6 Hz
XZ/ZX Orientation; ASTM D150
 3.58
@Frequency 1000 Hz
XY Orientation; ASTM D150
 3.73
@Frequency 1000 Hz
XZ/ZX Orientation; ASTM D150
Dissipation Factor 0.012
@Frequency 2.00e+6 Hz
XZ/ZX Orientation; ASTM D150
 0.013
@Frequency 1000 Hz
XY Orientation; ASTM D150
 0.014
@Frequency 1000 Hz
XZ/ZX Orientation; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°CXY Orientation; ASTM E831
 113 µm/m-°CXZ/ZX Orientation; ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CXY Orientation; ASTM D648 Method B
 90.0 °CXZ/ZX Orientation; ASTM D648 Method B
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CXY Orientation; ASTM D648 Method B
 70.0 °CXZ/ZX Orientation; ASTM D648 Method B
Glass Transition Temp, Tg 117 °CInflection Point, XY Orientation; ASTM D7426
 117 °CInflection Point, XZ/ZX; ASTM D7426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTRAS914 / 255808

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.