Key Features: - One component, no mix system
- Fast setting
- Rapid fixture time
- Non-toxic as per ISO 10993-5
Product Description: Master Bond MB297FLNT is a rubber toughened, single component ethyl cyanoacrylate system. Cyanoacrylates are commonly referred to as super glues or instant adhesives. MB297FLNT is a rapid curing, high strength compound used primarily in applications where ISO 10993-5 is specified. MB297FLNT has a low viscosity of 130-150 cps. This adhesive requires no mixing or heating, with minimal fixturing time for curing (typically 20-40 seconds). The most special feature of this system is its toughness. The rubber additive in the formulation mitigates the inherent stiffness of this cyanoacrylate system allowing for better thermal cycling and enhanced vibration resistance. MB297FLNT bonds well to a variety of substrates such as metals, composites, plastics and rubbers, especially in the shear mode. The service temperature range is -60°F to +250°F. MB297FLNT can be used in various applications ranging from field repair to high speed production. It has first rate resistance to EtO and gamma sterilization processes. Although many of the applications for MB297FLNT involve disposable medical devices, it also can be utilized with reusable medical devices depending upon the service conditions and type of sterilization. Product Advantages: - Rapid curing, generally sets up within less than one minute
- No heating or mixing
- Contact pressure usually sufficient for fixturing
- Excellent resistance to EtO and gamma sterilization
- Passes ISO 10993-5
- Contains rubber additive for increased toughness
Information provided by Master Bond. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |