MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Materion Titanium Oxide (TiOx) Rotatable Sputtering Target for Glass Applications
Categories: Ceramic; Oxide; Titanium Oxide

Material Notes: Materion is a leading supplier of rotatable sputtering targets for large area glass coatings. Our high purity Titanium Oxide (TiOx) sputtering targets are specifically developed to produce low defect and high performance thin films.

Benefits

  • Special target geometry provides greater material utilization
  • Longer target life time reduces downtime for change outs and chamber maintenance
  • Pure TiOx with optimized microstructure for best homogeneity and sputtering performance on full target volume
  • Customized x-value possible
  • Custom designed special geometries available
Application: Glass, dielectric base layer, blocker layer

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 4.00 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.190 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.39 µin/in-°F
Thermal Conductivity 3.00 W/m-K
Melting Point 1800 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMATER912 / 323565

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.