MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL GTX™ Resin GTX4610 Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 4610 resin is a 10% glass reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This high performance injection moldable grade has a UL 5VA flame rating, non-brominated / non-chlorinated FR package, UL746C Outdoor Suitability rating of F1, excellent chemical resistance, high heat resistance, high flow, and is laser weldable. NORYL GTX4610 resin is an excellent candidate for a wide variety of electrical applications including connectors, sockets, sensors, terminal blocks and insulator components. NORYL GTX™ 4610 resin is also an excellent candidate for electric vehicle (EV) battery applications including housings and covers.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Flame Retardant,Good Stiffness,Weatherable,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Moisture Absorption 0.0700 %0.0700 %Injection Molding
 0.500 %0.500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 3.8 %3.8 %ISO 62-1
Viscosity 15 cP
@Load 5.00 kg,
Temperature 300 °C
15 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0088 - 0.0094 cm/cm
@Thickness 3.20 mm
0.0088 - 0.0094 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0095 - 0.0101 cm/cm
@Thickness 3.20 mm
0.0095 - 0.0101 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 300 °C
18 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 88.0 MPa12800 psi5 mm/min; ASTM D638
 88.0 MPa12800 psi5 mm/min; ISO 527
Tensile Strength, Yield 88.0 MPa12800 psi5 mm/min; ASTM D638
 88.0 MPa12800 psi5 mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5 mm/min; ASTM D638
 3.0 %3.0 %5 mm/min; ISO 527
Elongation at Yield 3.0 %3.0 %5 mm/min; ASTM D638
 3.0 %3.0 %5 mm/min; ISO 527
Tensile Modulus 5.00 GPa725 ksi5 mm/min; ASTM D638
 5.00 GPa725 ksi1 mm/min; ISO 527
Flexural Strength 145 MPa21000 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 145 MPa21000 psiyield, 2 mm/min; ISO 178
Flexural Modulus 4.60 GPa667 ksi1.3 mm/min, 50 mm span; ASTM D790
 4.60 GPa667 ksi2 mm/min; ISO 178
Izod Impact Notched 80.0 J59.0 ft-lbASTM D256
 65.0 J
@Temperature -30.0 °C
47.9 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 12.0 J8.85 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Strength  23.2 kV/mm
@Thickness 1.60 mm
589 kV/in
@Thickness 0.0630 in
in air; ASTM D149
 24.4 kV/mm
@Thickness 1.60 mm
620 kV/in
@Thickness 0.0630 in
in oil; ASTM D149
Comparative Tracking Index 425 V425 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  41.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
22.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 41.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
22.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 224 °C435 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 220 °C
@Thickness 3.20 mm
428 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 218 °C424 °FRate B/50; ASTM D1525
 218 °C424 °FRate B/50; ISO 306
 220 °C428 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 305 °C536 - 581 °F
Zone 2 270 - 305 °C518 - 581 °F
Zone 3 275 - 305 °C527 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 75.0 - 120 °C167 - 248 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %minimum
Back Pressure 0.300 - 1.40 MPa43.5 - 203 psi
Shot Size 30 - 50 %30 - 50 %
Vent Depth 0.00130 - 0.00380 cm0.000512 - 0.00150 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82118 / 290065

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.