MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Copper Alloy, UNS C15730, H50 Temper, Rod & Bar
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extruded and Drawn

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked; Good Suitability – Soldering, Brazing; Poor Suitability – Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.66 g/cc0.313 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 120 - 135
@Load 0.500 kg
120 - 135
@Load 1.10 lb
Tensile Strength 359 - 400 MPa52000 - 58000 psi
 379 MPa55000 psiTypical
Tensile Strength, Yield 296 - 338 MPa43000 - 49000 psi0.2% Offset
 317 MPa46000 psiTypical, 0.2% Offset
Elongation at Break 15 - 20 %15 - 20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 ohm-cm0.00000200 ohm-cm88% IACS
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 1083 °C<= 1981 °F
Liquidus 1083 °C1981 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.26 - 0.34 %0.26 - 0.34 %
Boron, B <= 0.22 %<= 0.22 %
Copper, Cu >= 98.94 %>= 98.94 %
Iron, Fe <= 0.040 %<= 0.040 %
Oxygen, O 0.32 - 0.46 %0.32 - 0.46 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC15730x2 / 291579

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.