MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem HJSIL® R110 Treated Amorphous Hydrophobic Fumed Silica
Categories: Other Engineering Material

Material Notes: Product Description: Hjsil R110 is a kind of amorphous hydrophobic fumed silica, treated with poly dimethylsiloxane. Hjsil R110 is a high purity white colloidal powder.

Applications:

  • Adhesives and sealants
  • Composite materials
  • Glass-steels
  • Flake resins
  • Coatings and inks
  • Cable gels
  • Toner
Hjsil R110 can be used as thickener of plastic lubricants. It is used as thickening and thixotropy of complex polar liquids such as epoxy, polyurethane, or vinyl ester resins. In adhesives compounding, silica provides an additional method of promoting improved adhesion, as well as providing reinforcement. Hjsil R110 is used as an anticaking agent for powders.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 4.0 - 7.04.0 - 7.0suspension
Specific Surface Area 80 - 120 m²/g80 - 120 m²/gBET
 
Descriptive Properties
Appearancewhite colloidal powder
Content>99.8%SiO2, anhydrous bone-dry basis
Drying Loss<0.5%105°C, 2 hrs in oven

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH310 / 315228

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.