MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

KLJ Group KLJ PX 33 XLPE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: KLJ-PX-11 & 33 is based on Low Density, Cross Linkable Poly-Ethylene Compound for Continuous Vulcanization process to produce medium and high voltage power cable up to 33 KV.

Specifications: KLJ-PX-11 & 33 Compound meets the following specifications, when processed using sound extrusion and testing processes.

IEC-60502/60840., HD-620-S1, IS-7098 (Part-II)

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.922 g/cc0.922 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 15.0 - 18.0 MPa2180 - 2610 psiIS 10810 Part 7
 <= 21.6 MPa
@Treatment Temp. 132 - 138 °C,
Time 605000 sec
<= 3130 psi
@Treatment Temp. 270 - 280 °F,
Time 168 hour
IS 10810 Part 11
Elongation at Break >= 400 %>= 400 %IS 10810 Part 7
 <= 480 %
@Treatment Temp. 132 - 138 °C,
Time 605000 sec
<= 480 %
@Treatment Temp. 270 - 280 °F,
Time 168 hour
IS 10810 Part 11
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIS 3396
Dielectric Constant <= 2.2<= 2.2IEC 60250
Dielectric Strength >= 25.0 kV/mm>= 635 kV/inIEC 60243
Dissipation Factor <= 0.00040<= 0.00040IEC 60250
 
Descriptive Properties
Content200 ppmMoisture
Hot Set<65%200°C, 20 N/cm2, On molded sheet at 180°C for 20 minutes, IS 10810 Part-30
Permanent Set after cooling<5%IS 10810 Part-30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKLJ221 / 284242

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.