MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Vamac® G Ethylene Methacrylate (AEM)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Vamac® G is a terpolymer of ethylene, methylacrylate, and a cure site monomer cured using an amine-based vulcanization system. This gum elastomer includes a small amount of processing aid. It has excellent storage stability.

Vamac® G has excellent high-temperature durability and oil resistance with service lubricants, coupled with good low-temperature flexibility. Compounds of Vamac® G are typically rated at 175°C (347°F) for heat resistance, with oil swell values around 50% in ASTM No. 3 oil. These properties of Vamac® G make it well suited for a wide range of automotive applications, including powertrain seals and gaskets, rocker cover and piston seals, oil coolant hoses, power steering hoses, turbocharger hoses, crankcase ventilating tubes, coverings for fuel and coolant hoses, O-rings, grommets and spark plug boots.

Vamac® G is an excellent vibration damping material that is uniquely insensitive to temperature. Compounds of Vamac® G are suitable for use in torsional dampers and isolator pads.

Vamac® G is a halogen-free polymer and does not decompose to give off corrosive gases when exposed to flame. It is used for flame-retardant, low-smoke, nonhalogen wire and cable jackets and in nonhalogen, low-smoke flooring.

Vamac® G is well suited for injection, transfer and compression molding, and is easily extruded.

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
Volatiles <= 0.40 %EN 1400 / EN 14350-2
Mooney Viscosity 16.5
@Temperature 100 °C
ML 1+4; ISO 289-1-2
 40
@Temperature 100 °C
ML 1+4, Compound; ISO 289-1-2
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68ASTM D 2240
Tensile Stress at Strain 5.10 MPa
@Strain 100 %
ISO 527-1/-2
Compression Set 16 %
@Temperature 150 °C,
Time 252000 sec
ISO 815
 21 %
@Temperature 150 °C,
Time 605000 sec
ASTM D 395B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 175 °CDuPont proprietary test
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 °C
@Time 14400 sec
Cure Time 10.0 min
@Temperature 175 °C
 
Descriptive Properties
Colorclear to light yellow translucent
Part Marking Code>AEM<ISO 11469
Polymer(AEM)
Resin IdentificationAEMISO 1043
Scorch, Mooney viscosity> 16MS at 121°C; ISO 289-1-2
Scorch, time to 10 unit rise13MS at 121°C; ISO 289-1-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX4608 / 265818

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.