System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ LUBRICOMP™ Compound RX85514 Polyamide 66 (Nylon 66) (Europe)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
Material Notes:
LNP LUBRICOMP RX85514 compound is based on Nylon 6/6 resin containing proprietary fillers. Added features of this grade include: Wear Resistant.
Features: Wear resistant
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.29
g/cc
0.0466
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.012
-
0.014
cm/cm
0.012
-
0.014
in/in
SABIC method
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
71.0
MPa
10300
psi
5 mm/min; ISO 527
Tensile Strength, Yield
43.0
MPa
6240
psi
5 mm/min; ISO 527
Elongation at Break
5.3 %
5.3 %
5 mm/min; ISO 527
Elongation at Yield
3.3 %
3.3 %
5 mm/min; ISO 527
Tensile Modulus
3.80
GPa
551
ksi
1 mm/min; ISO 527
Flexural Strength
106
MPa
15400
psi
yield, 2 mm/min; ISO 178
Flexural Modulus
3.30
GPa
479
ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
4.00
kJ/m²
1.90
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
30.0
kJ/m²
14.3
ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
241
°C
466
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi)
97.0
°C
207
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH81046 / 288993
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.