MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL PPX™ Resin PPX630 Polyphenylene Ether + PP (PPE+PP) (Europe)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polypropylene (PP)

Material Notes: NORYL PPX™ 630 resin is a 30% glass reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade exhibits high elongation and high stiffness along with temperature performance, impact resistance, hydrolytic and dimensional stability. NORYL PPX630 resin is an excellent candidate for hot water system exteriors, condensate housings, and printer internals. *See NORYL PPX630F resin for NSF 61.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0400 %23°C / 50% RH
Water Absorption at Saturation 0.20 %ISO 62-1
Viscosity 3.0 cP
@Load 5.00 kg,
Temperature 260 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0020 - 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 75.0 MPaH358/30; ISO 2039-1
Tensile Strength at Break 80.0 MPa5 mm/min; ISO 527
Elongation at Break 4.1 %5 mm/min; ISO 527
Tensile Modulus 6600 MPa1 mm/min; ISO 527
Flexural Strength 120 MPabreak, 2mm/min; ISO 178
Flexural Modulus 5500 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 48.0 kJ/m²80*10*4; ISO 180/1U
 46.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 50.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 50.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.4
@Frequency 1e+6 Hz
IEC 60250
 2.4
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 24.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.00030
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 115 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 155 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 135 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 125 °CRate B/50; ISO 306
 128 °CRate B/120; ISO 306
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
Glow Wire Flammability Index 650 °C
@Thickness 3.20 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 260 - 300 °C
Zone 2 250 - 290 °C
Zone 3 255 - 290 °C
Melt Temperature 260 - 300 °CInjection Molding
Mold Temperature 40.0 - 65.0 °C
Drying Temperature 65.0 - 75.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82208 / 290155

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.