MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
A. Schulman Diamond Centrex® 825 Sheet Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it can be easily coextruded. The recommended substrate is ABS (acrylonitrile-butadiene-styrene) resin.

Applications: Typical applications for Centrex 825 resin includes exterior parts requiring high gloss, such as spas; marine components, boat hulls and decks; doors, covers, and trim for recreational vehicles; swimming pool steps; and fiberglass-reinforced plastic replacements. As with any product, use of Centrex 825 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Weatherable Polymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 97ASTM D785
Tensile Strength, Yield 33.8 MPachs 2.0 in/min; ASTM D638
Tensile Modulus 1700 MPachs 2.0 in/min; ASTM D638
Flexural Strength 50.3 MPachs 0.05 in/min; ASTM D790
Flexural Modulus 1700 MPatangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 53.0 J/m
@Thickness 3.17 mm,
Temperature -30.0 °C
ASTM D256
 107 J/m
@Thickness 3.17 mm,
Temperature -18.0 °C
ASTM D256
 214 J/m
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256
Impact Test 12.0 J
@Temperature -30.0 °C
ASTM D3763
 27.0 J
@Temperature -18.0 °C
ASTM D3763
 38.0 J
@Temperature 23.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 99.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C0.125";; ASTM D648
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Gloss 80 - 90 %Formed; 60°; ASTM D523
 90 - 100 %Sheet; 60°; ASTM D523

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond Centrex® 485 Sheet Extrusion Grade
Mocom (ALBIS) ALTECH® ASA A 1000/128 UV ASA
Teknor Apex Monprene® SP-14966 Thermoplastic Elastomer
A. Schulman Diamond ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus
A. Schulman Diamond ASA S130

PDIAM356 / 126447

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.