MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC FLEX NORYL™ Resin WCV072 Polyphenylene Ether + TPE (PPE+TPE) (Asia)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyphenylene Ether/PPO

Material Notes: FLEX NORYL™ WCV072 resin is a flexible, non-reinforced extrusion grade of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE) with a Shore D Hardness rating of 72. FLEX NORYL WCV072 resin was developed for evaluation in automotive wire + cable applications requiring ISO6722 Class A or B. It exhibits ultra-thin wall capability, good scratch abrasion and pinch resistance, high dimensional stability, low shrinkage and warpage, very low water absorption, chemical resistance, and good dielectric strength. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

Features: Flexible,Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Good Processability,Ductile

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccASTM D792
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Wire Coating Extrusion
 0.0500 %0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.12 %0.12 %ISO 62-1
Viscosity 13 cP
@Load 5.00 kg,
Temperature 280 °C
13 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Melt Flow 13.8 g/10 min
@Load 5.00 kg,
Temperature 280 °C
13.8 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 41.0 MPa5950 psi50 mm/min; ASTM D638
 42.0 MPa6090 psi50 mm/min; ISO 527
Tensile Strength, Yield 43.0 MPa6240 psi50 mm/min; ASTM D638
 44.0 MPa6380 psi50 mm/min; ISO 527
Elongation at Break 46 %46 %50 mm/min; ISO 527
 83 %83 %50 mm/min; ASTM D638
Elongation at Yield 11 %11 %50 mm/min; ISO 527
 15 %15 %50 mm/min; ASTM D638
Tensile Modulus 1.71 GPa248 ksi50 mm/min; ASTM D638
 1.75 GPa254 ksi1 mm/min; ISO 527
Flexural Strength 53.0 MPa7690 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 59.0 MPa8560 psiyield, 2 mm/min; ISO 178
Flexural Modulus 1.55 GPa225 ksi1.3 mm/min, 50 mm span; ASTM D790
 1.74 GPa252 ksi2 mm/min; ISO 178
Izod Impact Notched 309 J228 ft-lbASTM D256
 67.0 J
@Temperature -30.0 °C
49.4 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 36.0 kJ/m²17.1 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 3.30 J/cm²15.7 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 45.0 J33.2 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 85.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  105 µm/m-°C
@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 111 µm/m-°C
@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C208 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 92.0 °C
@Thickness 3.20 mm
198 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 114 °C237 °FRate B/50; ASTM D1525
 114 °C237 °FRate B/50; ISO 306
 117 °C243 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 15.0 - 80.0 °C59.0 - 176 °FWater Bath Temperature
 250 - 285 °C482 - 545 °FNeck Temperature
Feed Temperature 210 - 260 °C410 - 500 °F
Middle Barrel Temperature 230 - 285 °C446 - 545 °F
Die Temperature 250 - 285 °C482 - 545 °FWire Coating Extrusion
Melt Temperature 250 - 285 °C482 - 545 °FWire Coating Extrusion
Head Temperature 250 - 285 °C482 - 545 °FCross-head Temperature
 250 - 285 °C482 - 545 °F
Wire Preheat Temperature 80.0 - 150 °C176 - 302 °F
Drying Temperature 60.0 - 80.0 °C140 - 176 °FWire Coating Extrusion
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourWire Coating Extrusion
 12.0 hour12.0 hourCumulative; Wire Coating Extrusion
Screw Speed 15 - 40 rpm15 - 40 rpm
 
Descriptive Properties
Cooling Water Air Gap100-200 mm
Extruder Length/Diameter Ratio (L/D)22:1 to 26:1
Screen Pack150-100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82109 / 290056

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.