MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller 1925 Sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 1925 is a high quality, multi-purpose, sag-resistant one-component polyurethane sealant. This material is condensation cure material. It is used for automobile manufacturing, shipping industry, container manufacture, heating and ventilation systems, a variety of maintenance and repair applications.

Features and Benefits:

  • Low odor
  • Outstanding weather and aging resistance
  • Paintable after cure
  • Non-corrosive
  • Adhesion to a variety of materials have good adhesion chemical media capability
  • Resistant to age hardening, providing a consistent durometer measurement
  • Good UV resistance, making it ideal for interior and exterior applications

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
Storage Temperature 8.00 - 28.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
Tensile Strength >= 2.00 MPaASTM D638
Elongation at Break 600 %ASTM D638
Tear Strength 12.0 kN/m
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °C
 120 °CShort Term
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 6.00 hourHandling Time, at 25°C and 50% R.H.
 40.0 - 70.0 minSkin Formation Time
 24.0 hour
@Thickness 3.00 mm
Full-cure
Shelf Life 9.00 Month
 
Descriptive Properties
ColorBlack, White, Grey
ConsistencyThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL130 / 316921

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.