MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)

Information provided by Eurostar. Eurostar is being acquired by Ascend Performance Materials in 2021. This trade name is no londer in use.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccASTM D792
Moisture Absorption 1.20 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 4.5 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cmon Tensile Bar; E2P method
Melt Flow 25 - 50 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 113ISO 2039-2
Tensile Strength at Break 170 MPa5 mm/min; ISO 527
Elongation at Break 3.0 %5 mm/min; ISO 527
Tensile Modulus 9400 MPa1 mm/min; ISO 527
Flexural Strength 260 MPa2 mm/min; ISO 178
Flexural Modulus 9000 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Temperature -30.0 °C
80x10x4; ISO 179/1eA
 8.00 kJ/m²
@Temperature -40.0 °C
80x10x4; ISO 179/1eA
 9.00 kJ/m²
@Temperature -20.0 °C
80x10x4; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
80x10x4; ISO 179/1eA
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature -30.0 °C
Edgew 80x10x4 sp=62; ISO 179/1eU
 75.0 kJ/m²
@Temperature 23.0 °C
Edgew 80x10x4 sp=62; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
Edgew 80x10x4 sp=62; ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
Edgew 80x10x4 sp=62; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+16 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
IEC 60250
 3.4
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 19.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.0068
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 400 VM; IEC 60112
 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Thermal Conductivity 0.330 W/m-KASTM E1530
Hot Ball Pressure Test 123 - 127 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 260 °CEdgew 120x10x4, sp=100 mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 248 °CEdgew 120x10x4, sp=100 mm; ISO 75/Ae
Vicat Softening Point 258 °CB/120; ISO 306
 260 °CB/50; ISO 306
UL RTI, Electrical 65.0 °C
UL RTI, Mechanical with Impact 65.0 °C
UL RTI, Mechanical without Impact 65.0 °C
Flammability, UL94 HB
@Thickness 0.750 mm
 HB
@Thickness 3.00 mm
Flame Spread 2.00 mm/min
@Thickness 3.00 mm
FMVSS Burning Speed
 6.00 mm/min
@Thickness 2.00 mm
FMVSS Burning Speed
Oxygen Index 25 %ISO 4589
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Zone 1 260 - 280 °C
Zone 2 270 - 280 °C
Zone 3 270 - 290 °C
Melt Temperature 270 - 290 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 75.0 - 85.0 °C
@Time 14400 - 21600 sec
Moisture Content 0.20 %

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6
PTS Trimid® N66-G33L 33% Glass Fiber Reinforced Lubed Nylon 6/6
Envalior Durethan® AKV 30 H2.0 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 30 H2.0 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned

PEUROSTA53 / 172067

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.