MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Westlake Plastics Ethylux® Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Ethylux® LDPE is a soft, flexible, lightweight plastic material, noted for its low temperature flexibility, toughness, and corrosion resistance. The polymer also has a wide range of appeal for food processing and packaging markets. Ethylux® LDPE has good chemical and impact resistance and is easy to fabricate and form. It is a highly flexible product and is used widely in orthotics and prosthetic, or where mobility without stress fatigue is desired. Ethylux® LDPE is also frequently used in consumer packaging, bags, bottles, and liners.

Industry: Chemical Process; Engineering

Colors Available: Natural

Attributes: Impact Resistance; Chemical Resistance; Food Contact

Shapes: Compression Sheet

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.919 g/cc0.919 g/ccASTM D792
Water Absorption 0.040 %
@Time 86400 sec
0.040 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4242ASTM D2240
Tensile Strength at Break 12.4 MPa1800 psiASTM D638
Elongation at Break 650 %650 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.63
@Frequency 60.0 Hz
2.63
@Frequency 60.0 Hz
ASTM D1502
Dielectric Strength 19.2 kV/mm
@Thickness 3.17 mm
488 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.0060
@Frequency 60.0 Hz
0.0060
@Frequency 60.0 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 48.9 °C120 °FASTM D648
Vicat Softening Point 85.0 °C185 °FASTM D1525
Brittleness Temperature -75.0 °C-103 °FASTM D746
Flammability, UL94 HBHB
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEST905 / 243161

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.