MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Domo TECHNYL® AR 218 V33 Black 34 N Nylon 66, 33% glass fiber, DRY
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: Polyamide 66, reinforced with 33% of glass fiber, containing recycled material, for injection molding, specially stabilized to improve its resistance to automotive cooling liquids.

Available in: North America

Product Applications: TECHNYL® AR 218 V33 BLACK 34N is particularly recommended for the injection molding of parts in permanent contact with cooling liquids in cars, such as: - cooling and heating radiator systems, header tanks, thermostat components, inlet/outlet pipes. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 170 MPaISO 527 Type 1A
Elongation at Break 2.8 %ISO 527 Type 1A
Tensile Modulus 10051 MPaISO 527 Type 1A
Flexural Strength 258 MPaISO 178
Flexural Modulus 9015 MPaISO 178
Izod Impact, Notched (ISO) 8.20 kJ/m²ISO 180/1A
Charpy Impact Unnotched 48.6 kJ/m²ISO 179/1eU
Charpy Impact, Notched 7.80 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 11357
 
Processing PropertiesOriginal ValueComments
Feed Temperature 260 - 270 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50
Domo Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0

PRHOD548 / 137779

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.