MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cossa Polimeri ESTABLEND 4500 V0 HF Flame Retardant PC - ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PC - ABS Blend

Flame retardant class V0, chlorine and bromine free, good light resistance, excellent mechanical properties, excellent processability

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D 955
Melt Flow 30 g/10 min
@Load 5.00 kg,
Temperature 240 °C
30 g/10 min
@Load 11.0 lb,
Temperature 464 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.0 MPa6960 psiASTM D 638
Tensile Strength, Yield 50.0 MPa7250 psiASTM D 638
Elongation at Break 40 %40 %ASTM D 638
Flexural Modulus 2.60 GPa377 ksiASTM D 790
Izod Impact, Notched  5.00 J/cm
@Temperature 0.000 °C
9.37 ft-lb/in
@Temperature 32.0 °F
ASTM D 638
 5.50 J/cm
@Temperature 23.0 °C
10.3 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point  94.0 °C
@Load 5.00 kg
201 °F
@Load 11.0 lb
50°C/hr; ASTM D 1525
 105 °C
@Load 0.999 kg
221 °F
@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Glow Wire Test 960 °C1760 °FI.E.C. 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-ABS 802 Utility Grade White
Covestro Makrolon® 2207 Polycarbonate, Injection Grade
Covestro Bayblend® FR3110 TV PC/ABS Blend
Covestro Bayblend® FR3000 PC/ABS Blend
Cossa Polimeri ESTACARB 1560 V0 Flame Retardant Polycarbonate

PCOSSA895 / 156485

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.