MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin PKN4752 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL PKN4752 resin is a non-reinforced, translucent, high heat blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This extrudable and injection moldable grade exhibits high heat resistance, dimensional stability, and appears translucent with a yellow tint in the natural color. NORYL PKN4752 resin is an excellent candidate for high performance packaging in food, electronics, and healthcare. *See NORYL PKN4752F resin for FDA food compliant version.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Translucent,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 86.0 MPa50 mm/min; ISO 527
Elongation at Break 6.0 %50 mm/min; ISO 527
Tensile Modulus 3100 MPa1 mm/min; ISO 527
Flexural Strength 130 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2950 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²80*10*4; ISO 180/1A
 3.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 2.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 163 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 147 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 174 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CCalibrator Temperature
Zone 1 215 - 240 °CProfile Extrusion
Zone 2 225 - 250 °CProfile Extrusion
Zone 3 250 - 275 °CProfile Extrusion
Zone 4 250 - 275 °CProfile Extrusion
Adapter Temperature 250 - 275 °CProfile Extrusion
Die Temperature 250 - 275 °CProfile Extrusion
Melt Temperature 280 - 300 °CProfile Extrusion
Drying Temperature 80.0 - 95.0 °CProfile Extrusion
Dry Time 2.00 - 4.00 hourProfile Extrusion
Precipitation Temperature 50.0 - 70.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82416 / 290363

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.