MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Greene Tweed Arlon® 1000 Polyketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprietary manufacturing and machining processes to ensure that Arlons properties consistently outperform the competition.

Greene, Tweed offers several different Arlon materials, and all provide high tensile strength and elongation properties, excellent shear strength and creep resistance, outstanding fatigue resistance, broad chemical and radiation resistance, and no susceptibility to hydrolysis (steam/hot water). Our engineers work one on one with customers to find the right solution for each specific application.

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
Deformation 0.090 %0.090 %ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 104104ASTM D785
Hardness, Shore D 8888ASTM D2240
Tensile Strength at Break 96.5 MPa14000 psiASTM D368
 29.6 MPa
@Temperature 316 °C
4300 psi
@Temperature 600 °F
Tensile Strength, Ultimate 51.7 MPa
@Temperature 149 °C
7500 psi
@Temperature 300 °F
Tensile Strength, Yield 108 MPa15600 psiASTM D638
Elongation at Break 35 %35 %ASTM D638
Flexural Strength 174 MPa25300 psiASTM D790
 4.83 MPa
@Temperature 316 °C
700 psi
@Temperature 600 °F
 72.4 MPa
@Temperature 149 °C
10500 psi
@Temperature 300 °F
Flexural Modulus 4.14 GPa
@Strain 0.5 %
600 ksi
@Strain 0.5 %
Secant; ASTM D790
Compressive Strength 131 MPa19000 psiASTM D695
Shear Strength 85.5 MPa12400 psiAxial; ASTM D732
 85.5 MPa12400 psiTransverse; ASTM D732
 15.9 MPa
@Temperature 316 °C
2300 psi
@Temperature 600 °F
 46.9 MPa
@Temperature 149 °C
6800 psi
@Temperature 300 °F
Secant Modulus 4.24 GPa615 ksiTensile 0.5% Secant Modulus; ASTM D638
Coefficient of Friction, Dynamic 0.290.29PV=12600 psi-ft/min.; ASTM G77
K (wear) Factor 105 x 10-8 mm³/N-M52.0 x 10-10 in³-min/ft-lb-hrASTM G77
 
Thermal PropertiesMetricEnglishComments
CTE, linear  46.8 µm/m-°C
@Temperature <=149 °C
26.0 µin/in-°F
@Temperature <=300 °F
ASTM E228
 135 µm/m-°C
@Temperature >=149 °C
75.0 µin/in-°F
@Temperature >=300 °F
ASTM E228
Deflection Temperature at 1.8 MPa (264 psi) 177 °C350 °F
 
Descriptive Properties
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
VICTREX™ PEEK 450G™ General Purpose
Akro-Plastic Akrotek® PEEK natural (5184) PEEK, Dry
Barlog Plastics KEBAPEAK XS1700 PEEK, unreinforced
Greene Tweed Arlon® 2000 Polyketone

PGREEN49 / 42343

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.