MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BCC Products BX-51 Urethane Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Applications: BX-51 is used to make molds of masters that contain minor undercuts. BX-51’s physical properties make it ideal for making concrete patterns and formliners. BX-51 has been formulated to reduce shrinkage.

Characteristics: BX-51 is a two-part polyurethane molding system. BX-51 is mixed 100:97 by weight (or 1 Part-A Iso to 1 Part-B Curative by volume) and cures at room temperature. BX-51 cures to a medium hardness, Shore A 51± 2, gray rubber. Ultimate properties are obtained after 3-4 days of room temperature cure. Cure can be accelerated with heat (130-150°F for 12-16 hours) but a slightly harder polymer (53 +/- 2 Shore A) and slight shrinkage will be obtained.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.377 lb/galCurative (Part B)
 8.655 lb/galIso (Part A)
Viscosity 350 cPCurative (Part B)
 1000 cPIso (Part A)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 49 - 53
Tensile Strength 700 psiASTM D412
Elongation at Break 650 %ASTM D412
Tear Strength 23.0 plisplit; ASTM D470
 110 pliDie C; ASTM D624-C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 minMix Time
 24.0 hourDemold Time
 72.0 hourComplete Cure Time
Pot Life 15.0 - 25.0 min
Gel Time 12.0 - 14.0 min
Shelf Life 6.00 MonthIso (Part A)
 6.00 MonthCurative (Part B)
 
Descriptive Properties
ColorClear light yellow to amberIso (Part A)
 Opaque grayCurative (Part B)
Mix ratio100:97Iso (Part A):Curative (Part B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBCC115 / 250980

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.