Lupolen 2420 F is a non-additivated, low density polyethylene. It is characterized by a good melt strength leading to a good bubble stability during blown film extrusion. It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications :Agriculture Film, Bags & Pouches, Food Packaging Film, Hygiene Film, Liner Film, Shrink Film |