MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Ketjenblack EC-300J Electroconductive carbon black
Categories: Other Engineering Material

Material Notes: Pure electroconductive carbon black extremely suitable for antistatic and electroconductive applications.

CAS number: 1333-86-4

EINECS/ELINCS No: 215-609-9

Applications: Ketjenblack EC-300J is a very pure carbon black extremely suitable for antistatic and electroconductive applications. Due to its unique morphology and the very high surface area of approx. 800 m2/g (BET), only one third the amount of Ketjenblack EC-300J is needed compared to conventional electroconductive blacks in order to achieve the same conductivity. The lower loading of Ketjenblack EC-300J allows easier processing for those polymers sensitive to filler addition, thus minimizing loss in mechanical and rheological properties. Ketjenblack EC-300J when thoroughly dispersed with the polymer significantly increases the conductivity of the resulting compound. Ketjenblack EC-300J can be used in all types of polymers, thermoset, thermoplastic as well as elastomers. Due to its unique morphology and structure with relative low amounts of Ketjenblack EC-300J excellent conductive material can be made. The low grit content results in very smooth surfaces during extrusion. The loading needed to obtain a certain conductivity can vary significantly per type of polymer. More detailed information is provided in our special Ketjenblack EC Technical Bulletin. Ketjenblack EC-300J has a very low ash content, which makes it the preferred material for semicon applications in cable shielding. Ketjenblack EC-300J can also be used to produce conductive coatings and primers. Also here already at very low loading levels optimal electroconductive performance is obtained minimizing loss in mechanical and rheological properties. Some other applications are batteries, packaging for IC parts, tubing, flooring, carpet backing, automotive parts, cell phones and many more. For even more demanding applications Ketjenblack EC-600JD is available of which about half the amount is needed to obtain the same conductivity as with Ketjenblack EC-300J.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.125 - 0.145 g/cc0.00452 - 0.00524 lb/in³
Volatiles <= 1.0 %<= 1.0 %
Particle Size <= 125 µm<= 125 µm= 7%, Fines
pH 9.0 - 10.59.0 - 10.5
Ash <= 0.050 %<= 0.050 %
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %
 
Descriptive Properties
AppearanceBlack free-flowing pellets
Content= 30 mg/kgGrit content
 310-345 ml/100gPore volume, DBP
 740-840 mg/gIodine absorption

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY594 / 286117

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.