Characteristics: - Optical Grade
- The Most State of The Art form US NOVA CHEMICAL
- Low Residual Monomer
- Good Heat Resistance
- Mold Dimension Stability
- Good Transparency
- Easy Processing
- Good water resistance
Applications: - Diffuser of back light module.
Information provided by Taita Chemical Company, Limited |