MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Melos Mecoline IS RDX 5244 F Radiation cross-linkable VITON ® fluoro-elastomeric compound
Categories: Polymer; Thermoplastic

Material Notes: Radiation cross-linkable VITON ® fluoro-elastomeric compound

Compound class: Insulation / sheathing

Compound category: RDX

Flame retardant: Halogenated

Standards: ISO 6722-1 Class F

Typical applications: This modified fluoro-elastomer based compound is the right choice for manufacturing very flexible wires and cables. Applications in harsh environments in military, aerospace, automotive and other industries, where high performance takes first place.

Features: Flame retardant; Oil resistant; High temperature resistant; Flexible; Flexible at low temperatures

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³pressed plaques; DIN EN ISO 1183-1A
Melt Flow 12 g/10 min
@Load 21.6 kg,
Temperature 230 °C
12 g/10 min
@Load 47.6 lb,
Temperature 446 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7474pressed plaques; DIN ISO 7619-1
Tensile Strength 3.00 MPa435 psiextruded tapes; IEC 60811-501
 12.0 MPa1740 psicross-linked plaques or tapes; IEC 60811-501
Elongation at Break >= 200 %>= 200 %cross-linked plaques or tapes; IEC 60811-501
 450 %450 %extruded tapes; IEC 60811-501
 200 %
@Temperature 250 °C,
Time 605000 sec
200 %
@Temperature 482 °F,
Time 168 hour
cross-linked plaques / tapes, After ageing in air oven; IEC 60811-401
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmpressed plaques; ASTM D 257
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 225 °C437 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 215 - 225 °C419 - 437 °FTool
 250 °C482 °FMaximum mass temperature
Zone 1 180 - 190 °C356 - 374 °F
Zone 2 200 - 210 °C392 - 410 °F
Zone 3 210 - 220 °C410 - 428 °F
Zone 4 215 - 225 °C419 - 437 °F
Zone 5 215 - 225 °C419 - 437 °F
Adapter Temperature 215 - 225 °C419 - 437 °F
Head Temperature 215 - 225 °C419 - 437 °F
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 43 %43 %pressed plaques; ASTM D 2863 A
 
Descriptive Properties
Heat shockNo crackscross-linked plaques, at -70°C, ASTM D 2671C
Impact strengthNo crackscross-linked plaques, at -40°C, ASTM D 746
Main burning properties< 2 sec. after burnResistance to flame, ISO 6722

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS048 / 296155

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.