MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® V/T-2UV Low density moisture curable polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: PEXIDAN® V/T-2UV is a low density flame-retardant XLPE system curable by moisture and consists of a silane grafted base compound A-3001 and a catalyst masterbatch CAT-083FR-UV. Mixed and extruded in the proper proportions (50/50), the two components result in a material that is curable by exposure to hot water. PEXIDAN® V/T-2UV is halogenated but is RoHS-compliant. Insulation made with this system may be marked SUNRES or ‘SR’ in all colors and in all sizes per UL44, UL4703 and CSA C22.2 #38. This product is also CSA-listed for RW90, RWU90, RPV90 RPVU90 and CIC, ‘SR’ and -40C rated.

Information provided by SACO AEI Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Deformation 9.0 %UL 1581 / UL 2556
Storage Temperature <= 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1930 psiUL 1581 / UL 2556
 1950 psi
@Time 2.59e+6 sec
Weather-o-meter testing
 1790 psi
@Treatment Temp. 23.0 °C,
Time 2.59e+6 sec
After 30 day gasoline; UL 1581 / UL 2556
 1820 psi
@Treatment Temp. 75.0 °C,
Time 5.18e+6 sec
After 60 day oil; UL 1581 / UL 2556
 1950 psi
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; UL 1581 / UL 2556
Elongation at Break 300 %UL 1581 / UL 2556
 275 %
@Time 2.59e+6 sec
Weather-o-meter testing; UL 1581 / UL 2556
 290 %
@Treatment Temp. 75.0 °C,
Time 5.18e+6 sec
After 60 day oil; UL 1581 / UL 2556
 300 %
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; UL 1581 / UL 2556
 320 %
@Treatment Temp. 23.0 °C,
Time 2.59e+6 sec
After 30 day gasoline; UL 1581 / UL 2556
Crush Resistance 1360 lb (mass)UL 1581 / UL 2556
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.1
@Temperature 90.0 °C
UL 1581 / UL 2556
Dielectric Breakdown 21000 Vafter glancing impact; UL 1581 / UL 2556
 30000 VUL 1581 / UL 2556
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -60.0 °CASTM D746
Oxygen Index 27 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 310 - 340 °Fbarrel
Die Temperature 365 °F
Head Temperature 365 °F
 
Descriptive Properties
Degree of Crosslinking (%)60ASTM D2765
Hot Elongation Under Load (%)45SACO AEI DWI-QA-4007 based on ICEA T-28-562. 150°C/15 min.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO074 / 265504

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.