MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Eastar™ Renew EN076-30 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastar™ Renew EN076-30 copolyester is a sustainable, clear copolyester used in a variety of packaging and consumer product applications, including food & beverage packaging, general purpose packaging, flexible film packaging, and consumer products. It is fully compatible with the resin identification code 1 (RIC1) recycle stream. Eastar™ Renew EN076-30 copolyester enables fast-moving consumer goods brand owners to achieve recyclable products and packaging, reduce consumption of fossil-based resources, and replace materials of concern without sacrificing aesthetics or quality. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation. Eastar™ Renew EN076-30 copolyester meets the definition of resin identification code #1 (RIC1) as defined by ASTM D7611. Other end product attributes including but not limited to size, color, auxiliary components, and availability of collection may also impact recyclability. Eastar™ Renew EN076-30 copolyester may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED The GREENGUARD INDOOR AIR QUALITY CERTIFIED mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman™ Copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products.

Applications

  • Extruding
  • Mono-layer film food contact
  • Multi-layer film food contact
  • Packaging component - food contact
  • Packaging component films
  • Packaging components non food contact
  • Protective film
  • Transaction cards
  • Wood furniture
Key Attributes
  • Clear, bright, premium appearance
  • Easy to extrude
  • Great for film and rigid thermoform packaging
  • Not a material of concern
  • PVC alternative
  • Polystyrene (PS) alternative
  • Produced with ISCC certified circular content by mass balance allocation
  • Recyclable
  • Thermoformable

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ASTM D785
Flexural Modulus 2350 MPaASTM D790
Izod Impact, Notched 33.0 J/m
@Temperature -40.0 °C
ASTM D256
 67.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Optical PropertiesOriginal ValueComments
Haze 0.800 %ASTM D1003
Transmission, Visible 89.0 %Total; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 277 - 293 °C
Mold Temperature 16.0 - 32.0 °C
Drying Temperature 150 °C
Dry Time 4.00 - 6.00 hour
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details
 
Descriptive Properties
Bio-based ContentNone
Crystallization half time4.5 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4126 / 323749

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.