Product Description: PA 66, 15% Glass Fiber Reinforced, 25% Mineral Reinforced, Heat Stabilized, Lubricated, Post Industrial Recycled Feedstock, Black Color Availability: North America Filler/Reinforcement: Glass Fiber, 15% Filler by Weight; Mineral, 25% Filler by Weight Additive: Heat Stabilizer; Lubricant Recycled Content: Yes Features: Heat Stabilized; Lubricated RoSH Compliance: RoSH Compliant Automotive Specifications: GM GMW8751P-PA66-M25GF15 Color: Black Appearance: Black Information provided by Ravago Manufacturing Americas |