LNP STAT-KON DX05305C compound is based on Polycarbonate (PC) resin containing conductive carbon powder. Added features of this grade include: LNP Clean Compounding Technology, Low Ionic, Low Outgassing, Low LPC and Electrically Conductive. Features: LNP Clean Compound Technology,Electrically Conductive Information provided by SABIC |