MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC Xenoy® CL402U PBT+PC (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance performance. This grade is a CL402 with improved UV-performance.

This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
Moisture Absorption at Equilibrium 0.15 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.50 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cmon tensile bar; SABIC Method
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 250 °C
[cm^3/10 min] Melt Volume Rate; ISO 1133
 7.0 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, H358/30 85.0 MPaISO 2039-1
Tensile Strength, Yield 45.0 MPa50 mm/min; ISO 527
Elongation at Break 100 %50 mm/min; ISO 527
Elongation at Yield 4.0 %50 mm/min; ISO 527
Tensile Modulus 2000 MPa1 mm/min; ISO 527
Flexural Yield Strength 65.0 MPa2 mm/min; ISO 178
Flexural Modulus 1900 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 39.0 kJ/m²
@Temperature -40.0 °C
80*10*4; ISO 180/1A
 45.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 47.0 kJ/m²
@Temperature -20.0 °C
80*10*4; ISO 180/1A
 53.0 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 25.0 kJ/m²
@Temperature -30.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 40.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/2C
Taber Abrasion, mg/1000 Cycles 40
@Load 1.00 kg
CS-17; SABIC Method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.3
@Frequency 1e+6 Hz
IEC 60250
 3.3
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 18.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
Dissipation Factor 0.0020
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 105 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 105 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.190 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 105 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 123 °CRate B/50; ISO 306
 125 °CRate B/120; ISO 306
 155 °CRate A/50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94 by SABIC-IP
 
Descriptive Properties
Ball Pressure Test, 75°C +/- 2°CPASSESIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical Lupoy 1600-03 Polycarbonate Resin
Domo TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY
Celanese Riteflex® 830 TPC, Unfilled
Celanese FORTRON MT9205C4 PPS, Medical Technology
Celanese FORTRON 335 PPS, Unfilled

PSABIC6269 / 120157

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.