Product Description: NW-31 is a very fine white filler used for bulking and stiffening polymer systems, coatings, and sealing compounds. Flock improves impact and cut resistance; reduces shrinkage of molded parts. Nylon is less likely to absorb water than cotton flocks during service.Information provided by Akrochem Corporation |