MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Osterman & Co Osterlene® LD600-B LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD600 is a low density polyethylene resin. It’s a garment film resin with good toughness. It is capable of being drawn down to thing gauges.

Availability: North America
Additive: Antiblock: No; Slip:
Features: Good Drawdown; Good Toughness
Uses: Film
Processing Method: Blow Molding

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 230 %230 %ASTM D882
Film Elongation at Break, TD 480 %480 %ASTM D882
Secant Modulus, MD 0.180 GPa26.1 ksiASTM D790
Secant Modulus, TD 0.210 GPa30.5 ksiASTM D882
Elmendorf Tear Strength MD 400 g400 gASTM D1922
Elmendorf Tear Strength TD 180 g180 gASTM D1922
Dart Drop Test 70.0 g0.154 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 18.0 MPa2610 psiASTM D882
Film Tensile Strength at Break, TD 14.0 MPa2030 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 °C230 °FPeak; ASTM 3418
 
Optical PropertiesMetricEnglishComments
Haze 8.0 %8.0 %ASTM D1003
Gloss 70 %70 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POSTER077 / 267659

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.