MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC CYCOLAC™ MG94 ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Superior flow, injection molding ABS. Good impact. For thin-wall applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Viscosity 1720 cP
@Shear Rate 1000 1/s,
Temperature 240 °C
1720 cP
@Shear Rate 1000 1/s,
Temperature 464 °F
melt; ASTM D3825
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  11.7 g/10 min
@Load 3.80 kg,
Temperature 230 °C
11.7 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 12 g/10 min
@Load 5.00 kg,
Temperature 220 °C
12 g/10 min
@Load 11.0 lb,
Temperature 428 °F
ISO 1133
 42 g/10 min
@Load 10.0 kg,
Temperature 220 °C
42 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 113113ASTM D785
Tensile Strength at Break 35.0 MPa5080 psi50 mm/min; ISO 527
 35.0 MPa5080 psi5 mm/min; ASTM D638
Tensile Strength, Yield 46.0 MPa6670 psi50 mm/min; ISO 527
 46.0 MPa6670 psi5 mm/min; ASTM D638
Elongation at Break 18 %18 %5 mm/min; ASTM D638
 40 %40 %50 mm/min; ISO 527
Elongation at Yield 2.0 %2.0 %5 mm/min; ASTM D638
 2.3 %2.3 %50 mm/min; ISO 527
Tensile Modulus 2.45 GPa355 ksi1mm/min; ISO 527
 2.48 GPa360 ksi5 mm/min; ASTM D638
Flexural Yield Strength 70.0 MPa10200 psi2 mm/min; ISO 178
 79.0 MPa11500 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
 2.62 GPa380 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.40 J/cm4.50 ft-lb/inASTM D256
 0.800 J/cm
@Temperature -30.0 °C
1.50 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 21.0 J15.5 ft-lbASTM D3763
 5.00 J
@Temperature -30.0 °C
3.69 ft-lb
@Temperature -22.0 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  84.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 84.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 95.0 °C
@Thickness 3.20 mm
203 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C169 °F1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 82.0 °C
@Thickness 3.20 mm
180 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 98.0 °C208 °FRate B/50; ISO 306
 99.0 °C210 °FRate B/50; ASTM D1525
 100 °C212 °FRate B/120; ISO 306
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0598 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 205 - 245 °C401 - 473 °FInjection Molding
Zone 1 190 - 200 °C374 - 392 °F
Zone 2 200 - 210 °C392 - 410 °F
Zone 3 205 - 225 °C401 - 437 °F
Melt Temperature 205 - 245 °C401 - 473 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.10 %0.10 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 50 - 70 %50 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10106 / 243573

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.