MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ LUBRICOMP™ Compound DL003EU Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DL003EU compound is based on Polycarbonate (PC) resin containing 15% PTFE. Added features of this grade include: Easy Molding, UV Stabilized, Wear Resistant.

Features: Weatherable,Wear resistant,UV Resistant,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ASTM D792
 1.29 g/cc0.0466 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0080 - 0.0090 cm/cm0.0080 - 0.0090 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.0090 cm/cm0.0080 - 0.0090 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psiASTM D638
 50.0 MPa7250 psiISO 527
Tensile Strength, Yield 45.0 MPa6530 psiASTM D638
 54.0 MPa7830 psiISO 527
Elongation at Break 9.6 %9.6 %ISO 527
 25.5 %25.5 %ASTM D638
Elongation at Yield 5.5 %5.5 %ISO 527
 5.6 %5.6 %ASTM D638
Tensile Modulus 2.18 GPa316 ksi50 mm/min; ASTM D638
 2.20 GPa319 ksi1 mm/min; ISO 527
Flexural Strength 82.0 MPa11900 psiASTM D790
 84.0 MPa12200 psiISO 178
Flexural Modulus 2.30 GPa334 ksiASTM D790
 2.30 GPa334 ksiISO 178
Izod Impact Notched 143 J105 ft-lbASTM D256
Izod Impact, Unnotched 21.36 J/cm40.02 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 16.0 kJ/m²7.61 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²47.6 ft-lb/in²80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.180.18ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.0700.070ASTM D3702 Modified: Manual
K (wear) Factor 121 x 10-8 mm³/N-M60.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  73.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 75.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 138 °C280 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 128 °C262 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 116 °C
@Thickness 3.20 mm
241 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 305 - 315 °C581 - 599 °F
Zone 3 310 - 320 °C590 - 608 °F
Melt Temperature 300 - 315 °C572 - 599 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80741 / 288688

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.