MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound DL003 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DL003 compound is based on Polycarbonate (PC) resin containing 15% PTFE. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccASTM D792
 1.28 g/ccISO 1183
Water Absorption 0.20 - 0.30 %
@Time 86400 sec
ASTM D570
 0.20 - 0.30 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.0200 %Injection Molding
 0.0500 - 0.200 %23°C/50% RH/24 hrs; ASTM D570
 0.0500 - 0.200 %23°C / 50% RH; ISO 62
Viscosity 5.8 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cmSABIC method
Melt Flow 6.2 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 51.0 MPa50 mm/min; ASTM D638
 54.0 MPa50 mm/min; ISO 527
Elongation at Break 20 %50 mm/min; ISO 527
 37.6 %50 mm/min; ASTM D638
Elongation at Yield 5.1 %50 mm/min; ISO 527
 6.1 %50 mm/min; ASTM D638
Tensile Modulus 2150 MPa50 mm/min; ASTM D638
 2200 MPa1 mm/min; ISO 527
Flexural Strength 81.0 MPa2 mm/min; ISO 178
 82.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2100 MPa2 mm/min; ISO 178
 2190 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 280 JASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 140 kJ/m²80*10*4; ISO 180/1U
Charpy Impact Unnotched 180 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 22.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 30.0 Jpeak; ASTM D3763
Impact Test 34.0 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.18ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.26ASTM D3702 Modified: Manual
K (wear) Factor 60.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 76.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 98.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 128 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 127 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 144 °CRate B/50; ASTM D1525
 144 °CRate B/120; ISO 306
 144 °CRate B/50; ISO 306
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 V-1
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 305 - 315 °C
Zone 3 310 - 320 °C
Melt Temperature 300 - 315 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80738 / 288685

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.