MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C15715, H04 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Cold Worked; Good Suitability – Brazing; Fair Suitability – Butt Weld; Poor Suitability – Spot Weld, Seam Weld, Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B  63
@Thickness 19.0 mm
63
@Thickness 0.750 in
 67
@Thickness 12.7 mm
67
@Thickness 0.500 in
 68
@Thickness 6.99 mm
68
@Thickness 0.275 in
Tensile Strength  427 MPa
@Thickness 19.0 mm
62000 psi
@Thickness 0.750 in
 455 MPa
@Thickness 12.7 mm
66000 psi
@Thickness 0.500 in
 496 MPa
@Thickness 6.99 mm
72000 psi
@Thickness 0.275 in
Tensile Strength, Yield  62.1 MPa
@Thickness 19.0 mm
9000 psi
@Thickness 0.750 in
0.2% Offset
 434 MPa
@Thickness 12.7 mm
63000 psi
@Thickness 0.500 in
0.2% Offset
 469 MPa
@Thickness 6.99 mm
68000 psi
@Thickness 0.275 in
0.2% Offset
Elongation at Break  19 %
@Thickness 6.99 mm
19 %
@Thickness 0.275 in
 21 %
@Thickness 12.7 mm
21 %
@Thickness 0.500 in
 24 %
@Thickness 19.0 mm
24 %
@Thickness 0.750 in
Tensile Modulus 117 GPa17000 ksi
Fatigue Strength 221 MPa
@Thickness 6.99 mm,
# of Cycles 1.00e+8
32000 psi
@Thickness 0.275 in,
# of Cycles 1.00e+8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000181 ohm-cm0.00000181 ohm-cm95% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.20 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 30.4 W/m-K211 BTU-in/hr-ft²-°F
Melting Point 1083 °C1981 °F
 
Descriptive Properties
Cold Work (%)550.75 in
 800.5 in
 940.275 in
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC15715x6 / 291574

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.