MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Akrochem AKROCHEM® ZINC OXIDE XF-MA
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Zinc Oxide XF-MA is an extremely fine particle size French Process Zinc Oxide made from high purity (99.99%) zinc metal.

Uses: Zinc Oxide XF-MA is a fine particle size oxide serving as a cure activator/additive in rubber compounding, adhesives and latex applications. It is specially developed for highest reactivity, viscosity, fineness, and purity. Being a French process zinc, it can be used in white and colored rubber articles, where a zinc oxide of good color and high chemical purity is desirable. It also finds use in plastics, can sealants, paints and coatings, and in food can liner coatings.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 5.60 g/ccASTM D153
Particle Mesh Size 325 Mesh99.99% passing; ASTM D4315
Specific Surface Area 9.0 m²/gASTM D4315
 
Descriptive Properties
Content0.999ZnO (Dry Basis), ASTM D3280
 10 ppmCd (Cadmium), ASTM D4075
 30 ppmPb (Lead), ASTM D4075
Heat Loss0.001ASTM D280

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH656 / 315574

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.