MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin 2310EPR Polyetherimide (PEI) (Americas)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Enhanced Electroplatability,Easy Flow,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Density 1.48 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.90 %ISO 62-1
Viscosity 12 cP
@Load 5.00 kg,
Temperature 360 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cmSABIC method
 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 11 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 160 MPaH358/30; ISO 2039-1
Tensile Strength at Break 158 MPa5 mm/min; ASTM D638
 160 MPa5 mm/min; ISO 527
Tensile Strength, Yield 158 MPa5 mm/min; ASTM D638
 160 MPa5 mm/min; ISO 527
Elongation at Break 2.0 %5 mm/min; ISO 527
 2.1 %5 mm/min; ASTM D638
Elongation at Yield 2.0 %5 mm/min; ISO 527
 2.1 %5 mm/min; ASTM D638
Tensile Modulus 8580 MPa5 mm/min; ASTM D638
 8970 MPa1 mm/min; ISO 527
Flexural Strength 210 MPayield, 2 mm/min; ISO 178
 228 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9140 MPa1.3 mm/min, 50 mm span; ASTM D790
 9500 MPa2 mm/min; ISO 178
Izod Impact Notched 85.0 JASTM D256
Izod Impact, Unnotched 450 J/mASTM D4812
Izod Impact, Notched (ISO) 10.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²80*10*4; ISO 180/1U
 35.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 30.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 35.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 9.00 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=0.400 mm
UL 746A
 15 - 30 sec
@Thickness >=0.750 mm
UL 746A
 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=0.400 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
 18.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 30.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
 30.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.310 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 207 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 205 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 208 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 196 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 201 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 205 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 212 °CRate B/50; ISO 306
 214 °CRate B/120; ISO 306
 217 °CRate B/50; ASTM D1525
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.400 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 2 340 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °CInjection Molding
Mold Temperature 135 - 165 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82620 / 290567

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.