MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sirmax Dafnetec® PPS G12 PPS, Glass fibers and mineral filler reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Glass fibers and mineral filler reinforced

Application: Injection Molding

Information provided by Sirmax®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.96 - 1.98 g/ccISO 1183
Water Absorption 0.020 %ISO 62
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 107ISO 2039-2
Tensile Strength at Break 120 MPa5 mm/min; ISO 527-2
Elongation at Break 1.4 %5 mm/min; ISO 527-2
Flexural Strength 180 MPa2 mm/min; ISO 178
Flexural Modulus 17500 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.60e+14 ohm-cmIEC 60093
Surface Resistance 4.00e+15 ohmIEC 60093
Dielectric Strength 14.0 kV/mmIEC 60243
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.450 W/m-Kthrough-plane; ISO 22007-2
Hot Ball Pressure Test >= 190 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 275 °CISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 265 °CISO 75/Af
Vicat Softening Point 255 °CB50; ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
Glow Wire Ignition Temperature 875 °C
@Thickness 1.00 mm
IEC 60695-2-13
 875 °C
@Thickness 2.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 295 - 345 °CISO 294
Mold Temperature 130 - 150 °CISO 294
Drying Temperature 130 - 150 °C
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIRMX033 / 281136

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.