MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ STAT-KON™ Compound DX99873C Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DX99873C compound is based on Polycarbonate (PC) resin containing 25% carbon fiber. Added features of this grade include: LNP Clean Compounding Technology, Electrically Conductive, High Flow, Dimensional Stability.

Features: LNP Clean Compound Technology,High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Good dimensional stability,High Flow,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.150 %0.150 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.00050 cm/cm0.00050 in/in24hrs; ISO 294
 0.0010 cm/cm0.0010 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/in24hrs; ASTM D955
 0.0040 cm/cm0.0040 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 99.0 MPa14400 psiISO 527
 104 MPa15100 psiASTM D638
Elongation at Break 1.6 %1.6 %ISO 527
 1.7 %1.7 %ASTM D638
Tensile Modulus 10.75 GPa1559 ksi50 mm/min; ASTM D638
 10.8 GPa1570 ksi1 mm/min; ISO 527
Flexural Strength 163 MPa23600 psiISO 178
 171 MPa24800 psiASTM D790
Flexural Modulus 9.25 GPa1340 ksiISO 178
 9.68 GPa1400 ksiASTM D790
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
Izod Impact, Unnotched 4.85 J/cm9.09 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 13.0 J9.59 ft-lbpeak; ASTM D3763
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 1.00e+6 ohm100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  25.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
14.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 25.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
14.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  37.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
20.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 37.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
21.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 139 °C282 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 138 °C
@Thickness 3.20 mm
280 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-2
@Thickness >=1.50 mm
V-2
@Thickness >=0.0591 in
UL 94
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81275 / 289222

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.